Zinkgasse 7b, 8020 Graz · info@nickelgrid.cloud

Failure analysis (NG-PM)

NG-PM-03 - Teardown with diffraction and micro-CT

The full post-mortem, in which non-destructive imaging comes before the destructive opening so that the internal geometry is captured while it is still intact. A micro-CT scan down to a nine-micrometre voxel finds winding faults, electrode overhang and gas pockets; diffraction on recovered punches names the phases the images cannot. The two are read together, position against phase, rather than stapled side by side as separate reports.

NG-PM-At a glance
Method code
NG-PM-03
Minimum sample
1 cell
Turnaround
3 weeks
Temperature
not applicable
Live section
the NG-PM-03 entry in the live catalogue
01Parameters
Standing parameters for method NG-PM-03.
ParameterValue
CT voxeldown to 9 µm on a wound cell
Scan orderbefore opening, to catch the geometry
Diffractionon recovered electrode punches
Mappingphase against position inside the cell
02Equipment
  • micro-CT scanner, 9 µm voxel
  • diffraction stage
  • argon glove box
03Detail

Scanning before opening matters because the act of unrolling a wound cell relaxes the exact geometry the scan was meant to record. The nine-micrometre voxel is a genuine limit and we state it plainly: anything finer is invisible to this scan, and a client chasing a sub-voxel crack is told so rather than sold an image that cannot resolve it. Diffraction is taken from punches at named positions, so a phase change can be tied to where in the cell it occurred instead of to the electrode taken as a whole.

04Deliverables
  • reconstructed CT volume slices
  • diffraction patterns with phase assignment
  • combined geometry-and-phase note
  • method sheet

Every method ships with its method sheet, which quotes the code NG-PM-03 and the exact parameters used for your job.

05Related methods

The NG-PM-03 sheet is one of nine in the registry on the methods page; cycling fade curves are plotted on the data page.