Nickelgrid Materials TestingIndependent contract laboratory · Graz

Cell cycling, impedance spectroscopy and post-mortem analysis of battery materials. No product of our own; we measure what other people make.

Zinkgasse 7b, 8020 Graz · info@nickelgrid.cloud

Terms used across the site

Glossary

Twenty terms that recur on the method pages, in the reports and in the dataset, defined the way this laboratory uses them. Where a definition touches a choice we have made, the methodology page carries the reasoning in full.

A–ZDefinitions
Apparent diffusion coefficient
A diffusion figure derived from a titration run, carrying the word apparent because it rests on an assumed particle geometry; reported as a curve against state of charge rather than a single number.
C-rate
A current expressed relative to nominal capacity, so that 1C would in principle empty the cell in an hour; fixed after formation and held for the run.
Calendar ageing
Loss of capacity that accrues with elapsed time while a cell sits on open circuit, independent of how many cycles it has done.
Capacity retention
Discharge capacity of a later cycle divided by the first post-formation cycle at the same rate and temperature, written as a percentage.
Coulombic efficiency
Discharge capacity divided by the charge capacity of the same cycle, quoted to four decimals and never taken across a reference-test cycle.
Coverage factor (k=2)
The multiplier applied to a standard uncertainty to widen it to roughly ninety-five per cent coverage; every uncertainty we quote uses k equal to two.
Cut-off voltage
The upper or lower terminal voltage at which a charge or discharge step ends; a two-millivolt error here feeds about a tenth of a per cent into capacity.
DCIR
Direct-current internal resistance, taken from the voltage step at the start of a current pulse, distinct from the resistances a spectrum resolves.
Depth of discharge
The fraction of capacity removed from a full cell, the complement of the state of charge it is left at.
Formation
The first few slow cycles that build the passivating layer on the electrodes; nominal capacity is read from the third of these at C/20.
Impedance spectroscopy
Measurement of a cell's response to a small alternating perturbation across frequency, separating ohmic, charge-transfer and diffusion behaviour.
Micro-CT
X-ray computed tomography at microscopic resolution, down to a nine-micrometre voxel on a wound cell, used before a teardown to catch the geometry intact.
Nominal capacity
The discharge capacity of the third formation cycle at C/20, used as the reference for every later figure, not the datasheet value.
Nyquist plot
The usual way of drawing an impedance spectrum, the imaginary part against the real part, where the charge-transfer arc appears as a semicircle.
Post-mortem
The destructive opening of a failed cell to document, layer by layer, where and how it failed; also called a teardown.
Rate capability
How much of its slow-rate capacity a cell still delivers as the current is raised, reported as a retained fraction at each step of a rate ladder.
Reference performance test
A periodic slow measurement at a fixed rate and temperature inserted into a run so that drift in the test conditions is separated from drift in the cell.
Replicate
One of several nominally identical cells measured together; three is our minimum, because a single cell can sit four per cent off its own batch median by cycle three hundred.
State of charge
How full a cell is, as a fraction of its capacity, the quantity held fixed during calendar ageing and stepped through during a titration.
Voxel
The three-dimensional pixel of a CT reconstruction; features finer than the voxel edge are simply invisible to the scan.

A term you expected and did not find is probably on the relevant method page; the registry is on the methods page.