Preparation (NG-PRP)
NG-PRP-02 - Electrode coating from supplied powder
A preparation step rather than a measurement, run so that powders from different sources can be cycled on a common footing. Supplied active powder is mixed into a slurry, cast at a controlled areal loading, dried on a recorded profile and punched into half-cells. The output is not a result but a set of comparable cells ready for one of the cycling methods.
- Method code
- NG-PRP-02
- Minimum sample
- 3 g powder
- Turnaround
- 5 working days
- Temperature
- not applicable
- Live section
- the NG-PRP-02 entry in the live catalogue
| Parameter | Value |
|---|---|
| Loading | a target areal loading agreed in advance |
| Binder | the standard formulation unless specified |
| Drying | a controlled, recorded profile |
| Output | punched half-cells ready to cycle |
- slurry mixer
- film coater with an adjustable gap
- calendar and punch
Comparability is the whole point of the method: two powders coated to the same loading in one session can be ranked against each other, while two cells coated months apart on different gaps cannot. We log the loading and the dried thickness for every batch, because a difference in those two numbers accounts for most apparent performance gaps that turn out to be coating gaps. This route makes half-cells against lithium metal, not full pouches, and it is deliberately not a path to pilot-line quantities.
- coated and punched half-cells
- loading and thickness record
- method sheet
Every method ships with its method sheet, which quotes the code NG-PRP-02 and the exact parameters used for your job.
The NG-PRP-02 sheet is one of nine in the registry on the methods page; cycling fade curves are plotted on the data page.